basement wall carbon brace case study

PROBLEM

This interior block basement wall was cracking in deflecting in over an inch in the corner.

SOLUTION

The wall was prepped, brace locations were marked, then crack was filled with Xtreme 4000 epoxy. 3′ horizontal ReGrid extensions were installed at each corner brace location, followed by the installation of four solid carbon corner braces.